I-Nickel & Nickel Alloys Alloy 20

Iqokwe njenge-UNS N08020, i-Alloy 20 (eyaziwa nangokuthi “Incoloy 020” noma “Incoloy 20”) iyingxubevange ye-nickel-iron-chromium enezengezo zethusi ne-molybdenum. Inokumelana nokugqwala okukhethekile ku-sulfuric acid, i-choloride stress-corrosion cracking, i-nitric acid, ne-phosphoric acid. I-alloy 20 ingaba lula ukushisa noma ifakwe ngendlela ebandayo kuma-valve, ukufakwa kwamapayipi, ama-flanges, ama-fasteners, amaphampu, amathangi, kanye nezingxenye zokushintsha ukushisa. Izinga lokushisa lokwakha elishisayo kufanele libe phakathi kuka-1400-2150°F [760-1175°C]. Imvamisa, ukwelashwa kokushisa kwe-annealing kufanele kwenziwe ebangeni lokushisa lika-1800-1850°F [982-1010°C]. I-alloy 20 isetshenziswa kabanzi ukukhiqiza uphethiloli, amakhemikhali e-organic & inorganic, ukucubungula imithi kanye nemboni yokudla.

 

1. Izidingo Zokubumba Amakhemikhali

I-Chemical Composition of Alloy 20,%
I-Nickel 32.0-38.0
I-Chromiun 19.0-21.0
Ithusi 3.0-4.0
I-Molybdenum 2.0-3.0
Insimbi Ibhalansi
Ikhabhoni ≤0.07
I-Niobium+tantalum 8*C-1.0
Mananganese ≤2.00
Phosphorus ≤0.045
Isibabule ≤0.035
I-silicon ≤1.00

2. Mechanical Properties of Alloy 20

I-ASTM B462 Alloy 20 (UNS N08020) ukufakwa komgunyathi namaflange akhiwe.

Amandla Okuqina, imiz. Amandla Esivuno, imiz. Elongation, min. I-Modulus Encane
Mpa ksi Mpa ksi % 103ksi I-Gpa
620 90 300 45 40 28 193

3. Izakhiwo zomzimba ze-alloy 20

Ukuminyana Ukushisa Okuthize Ukungazweli Kagesi I-Thermal Conductivity
g/cm3 J/kg.°C µΩ·m W/m.°C
8.08 500 1.08 12.3

4. Amafomu Omkhiqizo kanye Namazinga

Ifomu Lomkhiqizo Okujwayelekile
Induku, ibha kanye nocingo I-ASTM B473, B472, B462
Ipuleti, ishidi kanye nomdweshu I-ASTM A240, A480, B463, B906
Ipayipi elingenamthungo neshubhu I-ASTM B729, B829
Ipayipi elishiselwe I-ASTM B464, B775
Ishubhu elishiselwe I-ASTM B468, B751
Ukufakwa okushiselwe I-ASTM B366
Ama-flange akhiwe kanye nokufakwa komgunyathi I-ASTM B462, B472