Ukumiselwa ngokweMigangatho
Inombolo yentsimbi. | I-DIN | EN | AISI | I-JIS | ГОСТ |
1.2085 | - | - | - | / | / |
Ukuqulunqwa kwemichiza (kubunzima %)
C | Si | Mn | Cr | Mo | Ni | V | W | Abanye |
0.35 | max. 1.00 | max. 1.40 | 16.00 | - | - | - | - | S: 0.070 |
Inkcazo
Intsimbi engatyiwa yiMartensitic imelana nomhlwa. I-1.2085 yentsimbi ibonisa ukuxhathisa kwe-corrosion engcono kwimeko yokuqina kunye nomphezulu ophucuziweyo ukunika isibuko ukugqiba. Iipropathi: I-Magnetizable steelm elungileyo ukumelana noomatshini kunye nokuqina, okugqwesileyo kwimveliso yamacandelo ekufuneka exhathise kwiiplastiki ezinobundlongondlongo, isixhobo esilungileyo sobuchule sibulela kumxholo wesulfure, esilungele ukusebenza kwiatmosfera emanzi kunye nokufuma, ilungele ukupolisha, ukunxitywa kunye nobungqina bomhlwa, kwaye uzinzile kakhulu ngexesha lonyango lobushushu.
Usetyenziso
Zonke iintlobo zezixhobo zokusika - iibhloko zokufa kunye ne-die-blocks kwishishini leplastiki elifana ne-PVC, iimela, izikere, izixhobo zotyando, ukubumba ukuveliswa kweeplastiki, kunye nezixhobo zotyando kunye neegeyiji zokulinganisa.
Iimpawu ezibonakalayo (amaxabiso aphakathi) kwiqondo lobushushu eliphakathi
Imodyuli ye-elasticity [103 x N/mm2]: 212
Ubuninzi [g/cm3]: 7.65
I-Thermal conductivity [W/mK]: 18
Ukuxhathisa kombane [Ohm mm2/m]: 0.65
Umthamo wobushushu obuthile[J/gK]: 460
Makazi: Ewe
I-Coefficient of Linear Thermal Expansion 10-6 oC-1
20-100oC | 20-200oC | 20-300oC | 20-400oC | 20-500oC |
11.0 | 11.1 | 11.2 | 11.8 | 12.0 |
I-Soft Annealing
Fudumeza ukuya kuma-760-780oC, uphole kancinci. Oku kuya kuvelisa ubulukhuni beBrinell obungama-230.
Ukuqina
Ukufudumala: 800oC. Ukuqina ukusuka kubushushu be-1000-1050oC kulandelwa yioyile, okanye ibhafu yokupholisa yepolymer. Ubunzima emva kokucima i-51-55 HRC.
Ukufudumeza
Ubushushu bobushushu: 150-200oC.
Ukuqulunqa
Ubushushu bokwenza okushushu: 1050-850oC, ukupholisa kancinci.
Ubuchule
Ubuchule obuhle kakhulu.
Phawula