Inconel 625 inowanikwa muMega Mex nenzira ipi?
- Sheet
- Plate
- Bar
- Pipe & Tube (yakasungwa uye isina musono)
- Waya
Ndeapi maitiro eInconel 625?
- Kusimba kwepamusoro-kutsemuka
- Oxidation inoshingirira kusvika 1800°F
- Gomba remvura yegungwa uye mukaha unodzivirirwa nekuora
- Immune kune chloride ion stress corrosion cracking
- Kwete-magnetic
Kemikari Inoumbwa,%
Cr | Ni | Mo | Co + Nb | Ta | Al | Ti | C | Fe | Mn | Si | P | S |
---|---|---|---|---|---|---|---|---|---|---|---|---|
20.00-30.00 | Remainder | 8.0-10.0 | 1.0 max | 3.15-4.15 | .40 max | .40 max | .10 max | 5.0 max | .50 max | .50 max | .015 max | .015 max |
Ndeapi maapplication anoshandiswa Inconel 625?
- Ndege ducting masisitimu
- Aerospace
- Jet injini exhaust systems
- Engine thrust-reverser masisitimu
- Specialized mvura yegungwa michina
- Chemical process midziyo
Kugadzirwa neInconel 625
Alloy 625 ine yakanakisa kuumba uye welding maitiro. Inogona kunge yakaumbwa kana kupisa yakashanda ichipa tembiricha inochengetedzwa mukati meiyo 1800-2150 ° F. Zvakanaka, kudzora saizi yezviyo, kupedzisa kupisa kwekushanda kunofanirwa kuitwa pamucheto wakaderera wekushisa. Nekuda kweiyo yakanaka ductility, alloy 625 inogadzirwa zvakare nyore nekutonhora kushanda. Nekudaro, iyo alloy inoshanda-kuomesa nekukasira saka kurapwa kwepakati-kunealing kunogona kudiwa kune yakaoma chikamu chekugadzira maoparesheni. Kuti udzorere zvakanakisa chiyero chezvivakwa, zvese zvinopisa kana kutonhora zvakashanda zvikamu zvinofanirwa kuvharwa uye nekukurumidza kutonhora. Iyi nickel alloy inogona kugadzirwa nemhando mbiri uye otomatiki welding nzira, kusanganisira gasi tungsten arc, gasi simbi arc, erekitironi danda uye kuramba welding. Inoratidza zvakanaka kuzvidzora welding maitiro.
Kuti uwane rumwe ruzivo nezvekugadzira uye machining, tinya pano.
ASTM Specifications
Pipe Smls | Pipe Welded | Tube Smls | Tube Welded | Sheet/Ndiro | Bar | Forging | Fitting | Waya |
---|---|---|---|---|---|---|---|---|
B444 | B705 | B444 | B704 | B443 | B446 | - | - | - |
Mechanical Properties
Representative Tensile Properties, bar, 1800° F anneal
Temp° F | Tensile (psi) | .2% Goho (psi) | Elongation mu2 "(%) |
---|---|---|---|
70 | 144,000 | 84,000 | 44 |
400 | 134,000 | 66,000 | 45 |
600 | 132,000 | 63,000 | 42.5 |
800 | 131,500 | 61,000 | 45 |
1000 | 130,000 | 60,500 | 48 |
1200 | 119,000 | 60,000 | 34 |
1400 | 78,000 | 58,500 | 59 |
1600 | 40,000 | 39,000 | 117 |