Alloy % Ni Cr Mo Fe W Co C Mn Si V P S
C Min. itule 14.5 15 4 3
Oke. 16.5 17 7 4.5 2.5 0.08 1 1 0.35 0.04 0.03
C276 Min. itule 14.5 15 4 3
Oke. 16.5 17 7 4.5 2.5 0.01 1 0.08 0.35 0.04 0.03

Alloy C-276 Njirimara anụ ahụ

Njupụta 8.9g/cm³
Ebe mgbaze 1325-1370 ℃

Alloy C-276 Alloy m kacha n'ibu Njirimara n'ime ụlọ okpomọkụ

Alloy steeti Ike ọdụdọ
Rm N/mm²
Mpụta ike
R P0. 2N/mm²
Ogologo oge
5%
C/C276 690 283 40

Njirimara dị ka n'okpuru
1.Excellent corrosion iguzogide ọtụtụ mgbasa ozi corrosion na oxidation na mbelata gburugburu.
2.Excellent iguzogide pitting, crevice corrosion na nrụgide corrosion cracking arụmọrụ.

Alloy C-276 Metallurgical Ọdịdị
C276 bụ usoro lattice cubic dabere na ihu.

Alloy C-276 nguzogide corrosion
C276 alloy uwe maka ọtụtụ ụdị kemịkalụ usoro ụlọ ọrụ nke nwere oxidizing ọkara na reductant. Nnukwu molybdenum na chromium ọdịnaya na-eme ka ọ nwee ike iguzogide corrosion chloride, na tungsten na-eme ka ọ dịkwuo mma.C276 bụ otu n'ime ihe ole na ole nke nwere ike iguzogide corrosion nke ọtụtụ chlorine, hypochlorite na chlorine dioxide, alloy a nwere nnukwu ihe mgbochi corrosion na-eguzogide elu. ịta chlorate (iron chloride na ọla kọpa chloride).

Alloy C-276 Ngwa ubi
A na-eji C276 n'ọtụtụ ebe na ubi kemịkalụ na ubi petrifaction, dị ka mmewere nke chloride organic na catalyze system.This ihe karịsịa uwe maka gburugburu ebe okpomọkụ dị elu, acid na-adịghị ọcha na organic acid (dị ka formic acid na acetic acid), oké osimiri. mmiri corrosion gburugburu ebe obibi.

Alloy C-276 Ngwa ngwa ndị ọzọ
1. The digester na bleacher na ojiji nke akwụkwọ pulp na akwụkwọ eme ụlọ ọrụ.
Ụlọ elu 2.Absorption, re-heater na fan na usoro FGD.
3. Akụrụngwa na akụkụ na iji gburugburu gas acidic.
4. Acetic acid na anhydride mmeghachi omume generator
5. Sulfur acid jụrụ oyi

6.MDI
7.Nrụpụta na nhazi nke phosphoric acid adịghị ọcha.

 

 