C46200 C4621 HSn62-1 eten an kwiv retire rad sou ou
GB | ASTM | JIS |
HSn62-1 | C46200 | C4621 |
HSn90-1 | C41100 | - |
GB | Konpozisyon chimik (%) | |||||
Cu | Sn | Ni | Fe | Pb | Zn | |
HSn62-1 | 61.0-63.0 | 0.7-1.1 | 0.5 | 0.1 | 0.1 | Balans |
HSn90-1 | 88.0-91.0 | 0.25-0.75 | 0.5 | 0.1 | 0.03 | Balans |
ASTM | Konpozisyon chimik (%) | ||||
Cu | Pb | Fe | Sn | Zn | |
C46200 | 62.0-65.0 | 0.2 | 0.1 | 0.5-1.0 | Balans |
C41100 | 89.0-92.0 | 0.1 | 0.05 | 0.3-0.7 | Balans |
Klas | Klas | Tanperaman | Epesè/mm | Fòs rupture Rm / MPa | elongasyon A11.2/% |
GB | ASTM | plis pase | |||
HSn62-1 | C46200 | Y | 0.25-0.75 | 390 | 5 |
Tan poste: Oct-28-2020