GH3536 Superalloy (Hastelloy X alloy)

Short Description:

GH3536, UNS N06002, W-NR 2.4665 Nickel-Based Superalloy


  • FOB Price: US $0.5 - 9,999 / Piece
  • Min.Order Quantity: 100 Piece/Pieces
  • Supply Ability: 10000 Piece/Pieces per Month
  • Port: Shanghai, Ningbo ,Shenzhen
  • Delivery time: 7-10 days after confirming the order
  • Origin: China
  • Payment Term: T/T , L/C
  • Standard: ASTM,AISI,SUS,JIS,EN,DIN,GB, ASME,etc
  • Mill: Pocso/ Tisco/ Lisco/ Jisco/ Bao steel/ H Wang
  • Product Detail

    Technical Specification

    Product Package & Shipment

    Company Introduction

    Question & Answers

    Product Tags

    GH3536, UNS N06002, W-NR 2.4665 Nickel-Based Superalloy

     

    GH3536 is a nickel-based superalloy with high iron content, mainly reinforced by solid solution of chromium and molybdenum, with a density of 8.3g/cm3.The most well-known commercial grade of the same steel is Hastelloy ® X Alloy.

     

    National Standard

    CHINA GB/T 14992-2005 GH3536(GH536)
    AMERICA ASTM B572-2011 UNS N06002
    HAYNES HASTELLOY® X alloy
    JAPAN JIS H 4551-2000 NW6002NiCr21Fe18Mo9
    NIPPON YAKIN NAS HX
    GERMANY DIN 17744-2002 2.4665NiCr22Fe18Mo
    VDM Metals Nicrofer®4722 Coalloy X

     

    Component Specification

    GRADE GH3536 N06002 NW6002 2.4665
    C 0.05~0.15 0.05~0.15 0.05~0.15 0.05~0.15
    Si ≤1.00 ≤1.00 ≤1.00 ≤1.00
    Mn ≤1.00 ≤1.00 ≤1.00 ≤1.00
    P ≤0.025 ≤0.040 ≤0.040 ≤0.020
    S ≤0.015 ≤0.030 ≤0.030 ≤0.015
    Ni Remainder Other
    Cr 20.5~23.0 20.5~23.0 20.5~23.0 20.5~23.0
    Mo 8.0~10.0 8.0~10.0 8.0~10.0 8.0~10.0
    Fe 17.0~20.0 17.0~20.0 17.0~20.0 17.0~20.0
    Co 0.5~2.5 0.5~2.5 0.5~2.5 0.5~2.5
    W 0.2~1.0 0.2~1.0 0.2~1.0 0.2~1.0
    Al ≤0.50 ≤0.50
    Ti ≤0.15
    Cu ≤0.50 ≤0.50
    B ≤0.01 ≤0.01 ≤0.01

     

    Application:

    GH3536 alloy under the high temperature of 1200 ℃, still has a very high strength and oxidation resistance, combined with excellent forming and welding performance, and excellent resistance to stress corrosion cracking performance, is widely used in gas turbine, industrial furnace, heat treatment equipment and the process of nuclear components, such as gas turbine combustion cylinder, burner taper pipe, transition, spray rod, distillation and the chemical industry, muffle furnace, catalyst support grille, hearth baffle, pyrolysis operation and flash drier parts of pipes, etc.


  • Previous:
  • Next:

  • Material Grade

    Material ASTM A240 Standard 201, 304 304L 304H 309S 309H 310S 310H 316 316H 316L 316Ti 317 317L 321 321H 347 347H 409 410 410S 430 904L
    ASTM A480 Standard 302, s30215, s30452, s30615, 308, 309, 309Cb, 310, 310Cb, S32615,S33228, S38100, 304H, 309H, 310H, 316H, 309HCb, 310HCb, 321H,347H, 348H, S31060, N08811, N08020, N08367, N08810, N08904,N08926, S31277, S20161, S30600, S30601, S31254, S31266,S32050, S32654, S32053, S31727, S33228, S34565, S35315,S31200, S31803, S32001, S32550, S31260, S32003, S32101,S32205, S32304, S32506, S32520, S32750, S32760, S32900, S32906, S32950, S32974
    JIS 4304-2005 Standard SUS301L,SUS301J1,SUS302,SUS304, SUS304L, SUS316/316L, SUS309S, SUS310S, 3SUS21L, SUS347, SUS410L, SUS430, SUS630  
    JIS G4305 Standard SUS301, SUS301L, SUS301J1, SUS302B, SUS304, SUS304Cu,SUS304L, SUS304N1, SUS304N2, SUS304LN, SUS304J1, SUSJ2,SUS305, SUS309S, SUS310S, SUS312L, SUS315J1, SUS315J2,SUS316, SUS316L, SUS316N, SUS316LN, SUS316Ti, SUS316J1,SUS316J1L,SUS317, SUS317L, SUS317LN, SUS317J1, SUS317J2,SUS836L, SUS890L, SUS321, SUS347, SUSXM7, SUSXM15J1, SUS329J1, SUS329J3L, SUS329J4L, SUS405, SUS410L, SUS429, SUS430, SUS430LX, SUS430J1L, SUS434, SUS436L, SUS436J1L,SUS444, SUS445J1, SUS445J2, SUS447J1, SUSXM27, SUS403,SUS410, SUS410S, SUS420J1, SUS420J2, SUS440A

    Product Specification

    Finish Thickness Characteristics Applications
    No. 1 3.0mm~50.0mm Finished by hot-rolling, annealing and pickling, characterized by white pickled surface Chemical industry equipment, Industrial tanks
    No. 2B 0.3mm~6.0mm Finished by heat treatment, pickling after cold rolling, followed by skin pass line to be more brighter and smooth surface General Application Medical Instruments, Tableware
    No. BA (Bright Annealed) 0.5mm~2.0mm Bright heat treatment after cold rolling Kitchen utensil, kitchen ware, architectural purpose
    No. 4 0.4mm~3.0mm Polishing with No. 150 to No.180 mesh abrasives. The most popular finishes Milk & Food processing facilities, Hospital Equipment, Bath-tub
    No. 8 0.5mm~2.0mm A mirror-like reflective surface by polishing with finer abrasives over 800 mesh Reflector, Mirror, Interior-Exterior decoration forbuilding
    HL(Hair Line) 0.4mm~3.0mm Finished by continuous linear polishing Architectural purposes, escalators, kitchen ware vehicles

    Chemical Composition

    Grade

    C

    Si

    Mn

    P

    S

    Cr

    Ni

    Mo

    Ti

    N

    Cu

    Nb

    201

    ≤0.15

    ≤1.0

    5.50-7.50

    ≤0.05

    ≤0.03

    16.00-18.00

    3.50-5.50

    -

    -

    0.05-0.25

    -

    -

    202

    ≤0.15

    ≤1.0

    7.50-10.00

    ≤0.05

    ≤0.03

    17.00-19.00

    4.00-6.00

    -

    -

    0.05-0.25

    -

    -

    301

    ≤0.15

    ≤1.0

    ≤2.0

    ≤0.045

    ≤0.03

    16.00-18.00

    6.00-8.00

    -

    -

    ≤0.1

    -

    -

    302

    ≤0.15

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    17.00-19.00

    8.00-10.00

    -

    -

    ≤0.1

    -

    -

    303

    ≤0.15

    ≤1.0

    ≤2.0

    ≤0.2

    ≥0.15

    17.00-19.00

    8.00-10.00

    ≤0.6

    -

    ≤0.1

    -

    -

    304

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    17.00-19.00

    8.00-10.00

    -

    -

    -

    -

    -

    304L

    ≤0.03

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    18.00-20.00

    8.00-10.00

    -

    -

    -

    -

    -

    304H

    0.04-0.1

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    18.00-20.00

    8.00-10.00

    -

    -

    -

    -

    -

    304N

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    18.00-20.00

    8.00-10.00

    -

    -

    0.10-0.16

    -

    -

    304J1

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    18.00-20.00

    6.00-9.00

    -

    -

    -

    1.00-3.00

    -

    305

    ≤0.12

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    17.00-19.00

    10.50-13.00

    -

    -

    -

    -

    -

    309S

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    22.00-24.00

    12.00-15.00

    -

    -

    -

    -

    -

    310S

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    24.00-26.00

    19.00-22.00

    -

    -

    -

    -

    -

    316

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    16.00-18.00

    10.00-14.00

    2.00-3.00

    -

    -

    -

    -

    316L

    ≤0.03

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    16.00-18.00

    12.00-15.00

    2.00-3.00

    -

    -

    -

    -

    316H

    ≤0.1

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    16.00-18.00

    10.00-14.00

    2.00-3.00

    -

    -

    -

    -

    316N

    ≤0.03

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    16.00-18.00

    10.00-14.00

    2.00-3.00

    -

    0.10-0.16

    -

    -

    316Ti

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    16.00-19.00

    11.00-14.00

    2.00-3.00

    ≥5C

    -

    -

    -

    317L

    ≤0.03

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    18.00-20.00

    11.00-15.00

    3.00-4.00

    -

    -

    -

    -

    321

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    17.00-19.00

    9.00-12.00

    -

    5C-0.7

    -

    -

    -

    347

    ≤0.08

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    17.00-19.00

    9.00-12.00

    -

    -

    -

    -

    10C-1.10

    347H

    ≤0.1

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    17.00-19.00

    9.00-12.00

    -

    -

    -

    -

    8C-1.10

    2205

    ≤0.03

    ≤1.0

    ≤2.0

    ≤0.035

    ≤0.03

    21.00-24.00

    4.50-6.50

    2.50-3.50

    -

    0.08-0.20

    -

    -

    2507

    ≤0.03

    ≤0.8

    ≤1.2

    ≤0.035

    ≤0.02

    24.00-26.00

    6.00-8.00

    3.00-5.00

    -

    0.24-0.32

    -

    -

    904L

    ≤0.02

    ≤1.0

    ≤2.0

    ≤0.045

    ≤0.03

    19.00-23.00

    23.00-28.00

    4.00-5.00

    -

    -

    1.00-2.00

    -

    C276

    ≤0.02

    ≤0.05

    ≤1.0

    -

    -

    14.00-16.50

    Other

    -

    -

    -

    -

    -

    Monel400

    ≤0.3

    ≤0.5

    ≤2.0

    -

    ≤0.024

    -

    ≥63

    -

    -

    -

    28-34

    -

    409L

    ≤0.03

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    17.00-19.00

    -

    -

    -

    -

    -

    -

    410

    ≤0.15

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    11.50-13.50

    -

    -

    -

    -

    -

    -

    410L

    ≤0.03

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    11.50-13.50

    -

    -

    -

    -

    -

    -

    420J1

    0.16-0.25

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    12.00-14.00

    -

    -

    -

    -

    -

    -

    420J2

    0.26-0.40

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    12.00-14.00

    -

    -

    -

    -

    -

    -

    430

    ≤0.12

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    16.00-18.00

    -

    -

    -

    -

    -

    -

    436L

    ≤0.025

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    16.00-19.00

    -

    -

    -

    -

    -

    -

    439

    ≤0.03

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    16.00-18.00

    -

    -

    -

    -

    -

    -

    440A

    0.60-0.75

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    16.00-18.00

    -

    ≤0.75

    -

    -

    -

    -

    440B

    0.75-0.95

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    16.00-18.00

    -

    ≤0.75

    -

    -

    -

    -

    440C

    0.95-1.2

    ≤1.0

    ≤1.0

    ≤0.035

    ≤0.03

    16.00-18.00

    -

    ≤0.75

    -

    -

    -

    -

    441

    ≤0.03

    0.2-0.8

    ≤0.7

    ≤0.03

    ≤0.015

    17.50-18.50

    -

    ≤0.5

    0.1-0.5

    ≤0.025

    -

    0.3+3C-0.9

    We wrap the stainless steel products with anti-rust paper and steel rings to prevent damage.

     Identification labels are tagged accordingto standard specification or customer’s instructions. 

    Special packing is available as per customer’s requirement.

    Stainless Steel Coil Package

    cepheus stainless steel coil package (1)

    cepheus stainless steel coil package (2)

     

    Stainless Steel Sheet / Stainless Steel Plate Package

    cepheus stainless steel  sheet package (3)

    cepheus stainless steel plate 1_副本

     

    Stainless Steel Strip Package

    cepheus stainless steel  strip package (5)

    Shipment Package

    Cepheus Stainless Steel Shipment (1)

    Cepheus Stainless Steel Shipment (2)

    Cepheus Stainless Steel Shipment (3)

    Our company is based in Wuxi,  gathering city of industrial stainless steel in China.

    We specialized in stainless coils, sheets and plate, stainless steel pipe and fittings, stainless steel tubes, and also aluminum products and copper products.

    Our products have been highly praised by our clients from Europe, America, the Middle East, African and Southeast Asia. We will offer competitive products and comprehensive service to customers. 

    Stainless Steel Grade: 201, 202, 202cu, 204, 204cu, 303, 304, 304L, 308, 308L, 309, 309s, 310, 310s, 316, 316L, 321, 347, 410, 416, 420, 430, 430F, 440, 440c,

    Alloy Grade :Monel, Inconel, Hastolley, Duplex, Super Duplex, Titanium, Tantalum, High Speed Steel, Mild Steel, Aluminium, Alloy Steel, Carbon Steel, Special Nickel Alloys

     

    In form of : Round Bars, Square Bars, Hexagonal Bars, Flat Bars, Angles, Channels, Profiles, Wires, Wire Rods, Sheets, Plates, Seamless Pipes, ERW Pipes, Flanges, Fittings,etc.

    wuxi cepheus stainless steel (1)

     

    wuxi cepheus stainless steel (5)

    wuxi cepheus stainless steel (4)

    wuxi cepheus stainless steel (3)

     

    wuxi cepheus stainless steel (2)

     

    Q1: What is stainless?

    A: Stainless means no marks on the steel surface, or a kind of steel that is not damaged by air or water and that does not change color, spotless, resistant to staining, rusting, the corrosive effect of chemicals.

    Q2: Does stainless mean no rusting?

    A: No, stainless means not easy to get stained or rusty, it has speical ability to reisist staining, rusting and corrosion.

    Q3: Do you supply stainless steel sheets?

    A: Yes, we supply different types of stainless steel sheets, with thickness ranges from 0.3-3.0mm. and in different finishes.

    Q4: Do you accept cut to length service?

    A: Of course, customer’s satisfaction is our top priority.

    Q5: If i have a small order, do you accept small order?

    A: Not a problem, your concern is our concern, small quantities are accepted.

    Q6: How can you guarantee your product quality?

    A: First, from the very start, we have already implemented a spirit to their mind, that is quality is life, our professional workers and staffs will follow up every step till the goods packed well and shipped out.

    Q7: Will you pack the products?

    A: Professional people do professional packing, we have different types of packing optional to customers, economic one or better one.

    Q8: What do you need to know from customer before accurate quotation?

    A: For an accurate quotation, we need to know grade, thickness, size, surface finish, color and quantity of your order, and also the destination of the goods. Customized product information will be needed more, like drawing, layout and plan. Then we will offer competitive quotation with the above information.

    Q9: What kind of payment term you accpet?

    A: We accept T/T, West union, L/C.

    Q10: If this is a small order, will you delivery the goods to our agent?

    A: Yes, we are born to solve problems of our customers, we will get the goods safely to your agent’s warehouse and send you the pictures.

    Q11: Do you just make flat sheet? I want to make a fabrication for my new project.

    A:  No, we mainly produce stainless steel flat sheet surface treatment, at the same time, we manufacture customized metal finished product as per customer’s drawing and plan, our technician will take care of the rest.

    Q12: How many coutries you already exported ?
    A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Iran,
          Turkey, Jordan, etc.
    Q13: How can I get some samples?
    A: Small samples in store and can provide the samples for free. Catalgue is available, most
          patterns we have ready samples in stock. Customized samples will take about 5-7days.
    Q14: What is the delivery ?
    A: Sample order’s delivery time is 5- 7 days. Container orders are about 15-20 days.

    Q15: What is the application about your Products?
    A:  1.elevator door/cabin or and escalator’s side-wall.
          2.Wall cladding inside or outside meeting room/ restaurant.
          3.Facade when cladding over something, like columns in the lobby.
          4.Ceiling in the supermarket. 5.Decorative draws in some entertainment places.
    Q16: How long Can You Guarantee for This Product/Finish?
    A: Color guarantee for more than 10 years. Original materials quality certificate can
           be provided.

  • Related Products